Steel is strong, but it wants only one thing: to go back to rust. Everything you like about a steel chair or cabinet is a thin layer that prevents this: chromium, nickel, paint or a dark forged skin. After seventy or ninety years that layer is no longer flawless, and it does not have to be. With a soft cloth, little water and now and again a little wax you keep the layer that is still there, and the piece simply stays in use.
First this
This book is a help, not a guarantee. Every piece is different. Try every product and every method first on a small spot that does not show, and stop if anything changes. What you do is at your own risk: De Huiszwaluw cannot be held liable for damage. If a piece is valuable or very dear to you, ask a conservator first.
What you have at home
Steel and iron are silvery grey and magnetic. Tubular steel furniture from the 1920s and 1930s is nickel-plated or chromium-plated: a very thin layer of metal on the steel. As long as that layer is unbroken, the steel beneath does not rust. School and office furniture is usually made of sheet steel with a coat of paint, which is colour and protection in one. Wrought iron is almost pure iron shaped with the hammer, often with a dark, firm skin or an old layer of black paint.
What damages it
Damp does the most. Clean iron stays stable at a relative humidity of about 50 per cent. Above about 65 per cent all iron rusts. Water that runs into a tube, a seam or a screw hole stays there and rusts the piece from the inside. Salt is the second enemy: the salt on your hands and salty air on the coast.
Not all rust is bad. Stable rust is hard, sits tight and is blue-black to reddish brown; in a dry room it no longer changes. Flash rust is a thin, bright orange film. Pitting is more serious: where the chromium or nickel has a pinhole, the steel underneath rusts, and the rust pushes the plating up into blisters and flakes.
Dull chromium and rust specks
How museums do it. A museum begins dry, with a soft brush or cloth. Greasy dirt comes off with a lightly dampened cloth with demineralised water and a drop of pH-neutral soap, and the metal is rubbed dry straight away. Chromium is not polished and not abraded, because the layer is so thin. Clean chromium is given a thin coat of microcrystalline wax.
How it is often done too. Furniture makers recommend a cloth with warm water and a little washing-up liquid for chromium, and rubbing dry at once afterwards. If the chromium is still dull after that, dealers take a fine chrome polish or metal polish: a little on a soft cloth, rubbed out with light pressure. Do that once and after that once a year at most, because even the finest polish is abrasive. A thin coat of car wax or microcrystalline wax afterwards keeps moisture out. The risk: in a place where the chromium is already thin, you polish through it, and it does not come back.
How it is often done too. Craftsmen take light rust specks off chromium in two ways. The first is the very finest steel wool, 0000, with a few drops of thin oil: rub gently and stop as soon as the orange has gone. The second is a wad of aluminium foil that you wet with water and rub over the specks. Then wipe everything clean, dry it well and wax it, otherwise the rust is back in no time. It goes wrong with coarser steel wool, which scratches, on ‘chrome’ that is in fact a coat of paint, and in places where the chromium is blistering or flaking: there you rub it loose.
Old paint on school and office furniture
How museums do it. The first coat of paint from the factory tells you which colour and which sheen the maker chose, and so it is kept, worn patches and all. Paint is only dusted. Water comes near it only after a cotton bud in a hidden place has shown whether colour comes off. Flaking paint is not touched, and a loose flake goes into an envelope.
How it is often done too. At home and in the trade an old cabinet or school chair is first cleaned well with lukewarm water and a little washing-up liquid, with a soft cloth wrung out until it is almost dry. Rub each surface dry at once. After that it is waxed. Take a clear hard wax from a tin, apply it very thinly with a cloth, leave it for a quarter of an hour and buff with a soft cloth. The paint regains its depth and bare worn patches are protected against flash rust. On powdery or flaking paint the cloth takes colour and flakes with it, and then you keep to dusting.
Bare steel and wrought iron
How museums do it. Loose rust powder is brushed away dry with a soft natural-bristle brush, not down to the bright metal, because bright iron gets orange spots again at once. Then the iron is given a few drops of light machine oil on a cloth, or a thin coat of microcrystalline wax.
How it is often done too. Blacksmiths wax iron that is kept indoors. Take a hard, clear wax or beeswax from a tin, rub it in thinly with a cloth, leave it for a quarter of an hour and buff until almost nothing is left on the surface. Once a year is enough indoors. Rub a rust spot away first with fine steel wool and a drop of oil, and then wax it again. Wax does not keep water out: in a bathroom, kitchen or conservatory waxed iron rusts all the same.
When re-chroming or respraying is a waste
How museums do it. They do not. Anyone who has a piece re-chromed or resprayed trades the original layer for a new one, and that cannot be undone. The Centraal Museum in Utrecht had the rust removed from a chromium-plated tubular chair by Rietveld from 1932, large flakes of chromium fixed back in place and the steel waxed. The chair now carries clear traces of use, and that was the intention.
How it is often done too. In the trade pieces are re-chromed and resprayed, especially ordinary everyday furniture on which the chromium has gone over large areas or the paint has already been painted over once. It is a waste on a piece by a well-known designer or factory, on a first coat of paint that is still largely attached, and on chromium that is only dull or has specks: cleaning and wax do enough for that. If there is a later coat of paint on top, the first is often still underneath, and after blasting or stripping it is gone for good.
What is better left alone
Do not use a scouring pad, sandpaper, a wire brush or coarse steel wool on chromium, nickel or paint: you are through the layer before you notice. Do not use rust remover. It contains acid, which eats patches down to the bare metal. Do not chip rust layers off or burst blisters. And never have a piece of steel furniture blasted or stripped before you know what you are throwing away.
When to go to a conservator
Go to a conservator when new flakes or rust powder keep appearing under the piece, when the chromium blisters or lifts over large areas, or when the paint flakes or turns powdery. Go too when a tube or a weld has rusted through: do not sit on the chair any more.
Patina is not dirt
Chromium gone dull on the armrest, paint worn down to the steel where generations of pupils took hold of their chair, a dark skin on wrought ironwork: that is not dirt and not a fault. It is the life of the piece, and it makes it what it is. At De Huiszwaluw you will find pieces that already have a life behind them, and you are always welcome to ask us how best to care for yours. We ship worldwide.
Written by De Huiszwaluw